Printing here with eSun PLA at 215 C on a Prusa Mini, and there are lots of hairline strings.
What’s causing those strings? Temp too low?
Printing here with eSun PLA at 215 C on a Prusa Mini, and there are lots of hairline strings.
What’s causing those strings? Temp too low?
Try dehydrateding your pla first. Then try some of these other suggestions. If all else fails, these clean up really nicely with a butane blow torch.